E S H I O N

Aluminum Anodizing Explained

Aluminum Anodizing Explained

Aluminum anodizing is the finish most buyers add last and check least. Yet a coating only 10 to 50 microns thick can decide whether a bore accepts its bearing, whether two housings match in color, and whether a bracket survives a salt-laden warehouse.

This guide explains how anodizing works, how the three types differ, which coating thickness to call out, and how much the coating changes the size of a machined part. It also covers alloy limits, masking, alternative finishes, and what to check when you buy anodized parts in volume.

What Aluminum Anodizing Does to a Machined Part

Anodizing turns the outer layer of an aluminum part into aluminum oxide. Paint and powder coat sit on top of the metal. Anodic oxide grows from the metal itself, so it does not peel the way paint can.

The part acts as the anode in an acid bath. Current drives oxygen to the surface, and the oxide forms in two layers: a thin, dense barrier layer next to the metal and a thicker layer of microscopic pores above it. The pores matter. They hold dye, and a sealing step closes them afterward.

The oxide is hard, brittle and electrically insulating. Those three traits explain most of the design rules in this article.

Your supplier cleans and etches the part, anodizes it, dyes it if you want color, seals it, and inspects it. You influence each step: the surface you hand over, the type and thickness, the color, whether the pores are sealed, and how thickness is measured.

Anodizing also shows what lies under it. Tool marks stay visible. If the face is cosmetic, ask for bead blasting for a uniform matte surface, or a vibratory or grained finish, before the part goes into the tank.

Type I, Type II and Type III: Which Fits CNC Parts

Type Process Spec thickness range (MIL-A-8625F) Typical use on CNC parts
Type I Chromic acid 0.5–7.6 µm Rare; thin coating for fatigue-sensitive parts
Type II Sulfuric acid 1.8–25.4 µm Corrosion protection and color on housings, brackets, covers
Type III Hardcoat (sulfuric acid, cold bath, high current) 12.7–115 µm Wear surfaces: sliding faces, guides, clamps

Type I uses chromic acid, and environmental restrictions keep it uncommon. Most buyers of CNC parts never need it.

Type II is the standard choice. It protects against corrosion and takes dye well. The specification splits it into Class 1 (undyed) and Class 2 (dyed).

Type III builds a thicker, harder, darker coating. Its natural color runs from gray-brown to black, and it takes dye poorly because the pores are smaller.

The practical rule for Type II vs Type III anodizing is simple. Choose Type II unless the surface slides, rubs or abrades. Then choose Type III. Do not specify Type III for general protection. It costs more, grows more, limits color, and can shorten fatigue life.

Anodizing Thickness: Which Number to Put on Your Drawing

Sources quote different thicknesses because they mix three things: the limits the specification allows, the ranges shops run in practice, and the defaults a shop applies when the drawing says nothing.

The specification allows 1.8 to 25.4 µm for Type II, but dyed parts need more than the minimum. Dye needs roughly 10 to 15 µm of coating to hold color. One prototype manufacturer publishes ISO 7599 class AA10 (10 µm minimum average) for clear parts and AA15 (15 µm) for black and colored parts. For dyed Type II, 15 to 20 µm is a sound call-out.

For Type III, 50 µm (0.002 in) is the usual figure. Many finishers apply that default when the drawing is silent, which means your tolerances may not survive it.

Measure thickness with an eddy-current gauge (ASTM B244). The gauge reads coating thickness. It does not tell you how far the part grew. To measure growth, compare a finished part against an uncoated sample.

How Much Does Anodizing Change CNC Part Dimensions?

Anodizing consumes aluminum to make oxide. Part of the coating goes into the surface and part grows outward. Many guides use a half-and-half split for every type. Measured ratios differ: Type II grows outward by about one-third of its thickness (finishers cite 33 to 40%), and Type III by about half.

Take a Ø10.00 mm hole with a ±0.05 mm tolerance.

A 15 µm Type II coating adds about 5 to 6 µm per surface. The hole shrinks by 0.010 to 0.012 mm, to roughly Ø9.989. That uses about a fifth of the minus side of the tolerance.

A 50 µm Type III coating adds about 25 µm per surface. The hole shrinks by 0.050 mm, to Ø9.950. That lands exactly on the lower limit.

Shafts and pins grow by the same amount on the diameter. For ±0.05 mm parts, Type II usually fits inside the tolerance band. Type III never does without a plan.

You have three ways to handle it. State on the drawing that dimensions apply after anodizing, so the shop machines to compensate. Mask the feature. Or machine the feature after anodizing. Choose by function: a cosmetic cover can accept compensation, while a press-fit seat needs bare metal or a tightly controlled coating.

Alloy Choice Decides How the Finish Looks

The same tank gives different results on different alloys.

6061-T6 and 6063 anodize cleanly and accept the full range of dyes. 5052 gives a slightly grayer tone. 7075 shifts toward yellow, brown or olive-gray because of its zinc content, and 2xxx alloys with high copper come out dull and uneven.

Mixed-alloy assemblies cause the most disputes. A 7075 bracket and a 6061 housing sent through the same black bath come back as two different blacks. If appearance matters, use one alloy across the assembly or split the finish: black on the 6061 housing, and a function-first finish on the bracket.

Die-cast alloys are the hardest case. ADC12 contains 9.6 to 12% silicon, and silicon does not anodize. Expect gray, mottled or black-smutty results, and expect hardcoat to perform poorly. This affects sourcing decisions. A die-cast housing and a machined housing from wrought alloy will not look the same after anodizing, so a quote comparison between them is not like for like.

Alloy lots also vary. Slight composition differences between lots of the same grade can shift color, which makes exact matches across batches difficult.

Threads, Bores, Ground Contacts and Rack Marks

Guides disagree on threads. Some say mask every thread. Others say Type II leaves threads alone. Both can be right, depending on the thread and the coating.

Type II adds roughly 3 to 8 µm per surface, so many general-purpose threads survive it. Mask or chase the threads after coating when the thread is fine-pitch, the fit class is tight, the part is assembled repeatedly, or the thread seals or bonds electrically. On Type III, mask threads by default or cut them after coating.

Masking is hand labor. Every plugged hole and taped face adds cost, so mask only what function requires. Keeper brackets with metric or UNC threads show the trade-off: hole position and thread type decide whether the part fits, so those are the features to mark on the drawing.

The oxide insulates. If a face must ground or bond electrically, mask it or choose a different finish.

Parts hang on racks during anodizing, and the contact points stay bare. Pick a face where a bare mark is acceptable and write it on the drawing. If no face qualifies, tell the supplier so they can plan plugged-hole racking.

Benefits of Anodized Aluminum, and Where They Stop

Corrosion resistance

Sealing decides corrosion performance. The specification requires sealed Type II coatings to pass 336 hours of salt-spray testing. Type III sealing is optional, and an unsealed hardcoat gives up some corrosion protection to keep maximum abrasion resistance.

Wear resistance

Type III hardcoat typically measures 400 to 530 HV. One US finisher’s Taber testing puts it at about ten times the abrasion resistance of Type II. Type II resists wear better than bare aluminum, but it is not a sliding surface.

Appearance

Type II takes most colors, but matching a Pantone or RAL reference is unrealistic, because color varies with alloy lot and bath. Electrolytic coloring resists UV better than organic dye, which matters for outdoor parts. Type III stays in a narrow range of natural and black.

Heat dissipation

Bare polished aluminum has an emissivity around 0.04. A standard finishing handbook reports anodized 6061 at 0.70 to 0.72 with a 6 µm coating and 0.75 to 0.80 at 11 µm (clear and black). Supplier pages often quote 0.8 to 0.9 for black anodize. Treat the exact value with caution and test it if the design is thermally tight.

The gain shows mainly in natural convection. With forced air, convection dominates and the benefit shrinks. The film is only microns thick, so most designers treat its effect on conduction as small. A thick polymer coating, by contrast, adds insulation.

Limits to plan for

Thick hardcoat can cut fatigue life. Published reductions reach 30 to 50% on some high-strength alloys, so avoid it on parts that flex under repeated load. The coating insulates, so ground faces need masking. It also builds at sharp external edges, so ask your finisher for a minimum edge radius on hardcoated parts.

Anodizing vs Chem Film vs Powder Coating

Chem film (also called alodine or chromate conversion, specified under MIL-DTL-5541) keeps aluminum conductive and barely changes dimensions. Use it for grounding surfaces and EMI enclosures. It gives corrosion protection and a paint-ready surface, but little wear protection. Some shops also choose it for heat sinks that rely on conductive contact.

Powder coating gives thick, impact-resistant color, and it covers tool marks when you apply a vibratory finish first. The layer is thick enough to affect fits, and it insulates, so mask any contact face.

A short decision path works for most parts. Pick Type III for wear, Type II for corrosion and appearance, chem film for conductivity, and powder coat for impact and bold color on larger parts. You can combine finishes on one part. Hardcoat the wear bore and finish the rest with Type II or chem film, with masking between the zones.

Matching the Finish to the Part

Finned housings and enclosures. Specify 6061-T6 with dyed black or clear Type II at 15 to 20 µm. Mask any grounding pad, and confirm with your thermal engineer whether the design relies on radiation. A CNC machined aluminum housing with cooling fins is the typical example, and housing and cover sets add a mating face to protect.

Brackets and mounting plates. Clear Type II protects against corrosion. Mark threaded holes and locating bores for masking or compensation, since hole position and thread type decide fit.

Sliding and wear parts. Guides, locating pins and clamps in automated lines need Type III at about 50 µm. Add the growth to the drawing, and check fatigue if the part flexes. These parts often sit inside larger systems. Our post on custom automation solutions for modern manufacturing shows where such parts fit, and automation components gives product examples.

Cosmetic covers. Bead blast, then apply Type II in one alloy and, if possible, one lot. Approve a master sample before bulk production.

How to Specify Anodizing on a CNC Drawing

A complete call-out names the alloy and temper, the specification, type and class, color, thickness, sealing, masked features, the dimension basis, and the permitted rack-mark zone. Here are two examples. Adjust the values to your part’s function.

Housing, cosmetic and corrosion protection:
Material: 6061-T6. Anodize per MIL-A-8625, Type II, Class 2, black, 15–20 µm, sealed. Mask the four M6 threaded holes and the 20 × 20 mm ground pad. Dimensions apply after anodizing. Rack marks permitted inside the Ø8 mounting bore only.

Wear part:
Material: 6061-T6. Hard anodize per MIL-A-8625, Type III, Class 1, natural, 50 µm ±10 µm, unsealed. Mask the Ø12 H7 bore. All other dimensions apply after anodizing.

Suppliers also cite the same specification as MIL-PRF-8625, so either designation is recognized. An incomplete call-out forces the shop to guess. Type III’s 0.002 in default is the most common surprise.

Buying Anodized CNC Parts at Wholesale Volume

Compare quotes on the same finish specification

Two quotes mean nothing if one assumes 10 µm Type II and the other assumes 15 µm. Send the same call-out to every supplier, and ask each to state the thickness, class, sealing and masking they quoted.

Know what drives the price

Type and thickness set the base cost. Color, masking labor, racking constraints, alloy and quantity move it. Type III costs more than Type II, and the gap depends on thickness and masking, so ask for both quotes when you are unsure which you need.

Ask your supplier five questions

Who runs the anodizing line, the supplier or an outside shop? An outside shop adds a handoff and lead time. Which specification and class do they run to? How do they verify thickness, and do they provide a report? How do they handle growth on critical features? What color standard do they work to?

Keep color and fit consistent across batches

Approve a sample before bulk production and keep it as the reference. Buy cosmetic parts from as few alloy lots and bath batches as you can. Put the drawing revision on every purchase order. A prototype order catches a wrong finish or a fit problem when the fix costs one part, not a full order.

When you source wholesale CNC components, these checks protect you more than a lower unit price does. At Eshion, the listed CNC machined aluminum components ship anodized, powder coated or polished and hold ±0.05 mm. We confirm the finish type and whether your tolerance applies before or after finishing before we quote, and we make samples before bulk runs.

FAQs

Does anodized aluminum rust?

No. Rust is iron oxide, so the term does not apply to aluminum. Anodized parts can still corrode or stain in aggressive environments if the coating is thin, unsealed or scratched through, which is why thickness and sealing matter.

Can I match 7075 parts to 6061 parts in black?

Not exactly. 7075 shifts toward brown, so the two alloys give visibly different blacks. Use one alloy across the assembly, or accept the difference on non-visible parts.

Can one part carry both Type II and Type III?

Yes, with masking. A common example is hardcoat in a wear bore and Type II on the rest of the part.

Is anodized aluminum conductive?

No. The oxide insulates. Mask grounding faces, or use chem film where conductivity matters.

Send the Finish Call-Out With Your Drawing

A drawing that states type, class, thickness, sealing, masking and dimension basis gets a faster and more accurate quote. Send it with your alloy, quantity and delivery term, and we confirm each point against your CNC machined aluminum parts before we price them.

Featured Articles

11-Nov-2026 Aluminum Anodizing Explained

Aluminum anodizing is the finish most buyers add last and check least. Yet a coating only 10 to 5...

READ FULL
02-Sep-2026 From Prototype to Mass Production: Complete OEM & ODM Engineering Support

Developing a customized industrial product requires more than precision manufacturing—it re...

READ FULL
02-Sep-2026 Precision CNC Components for High-Performance Industrial Applications

Precision CNC machining plays a critical role in industries where accuracy, consistency, and reli...

READ FULL

Leave Your Comments